Mikrostrukturentwicklung beim Friction Stir Processing von Ti-6Al-4V

Claudia Ramskogler, Alfred Krumphals, Christof Sommitsch

Research output: Contribution to conferencePosterResearch

Original languageGerman
Publication statusPublished - 2011
EventASMET Forum - Leoben, Austria
Duration: 9 May 201110 May 2011

Conference

ConferenceASMET Forum
CityLeoben, Austria
Period9/05/1110/05/11

Fields of Expertise

  • Sonstiges

Treatment code (Nähere Zuordnung)

  • Basic - Fundamental (Grundlagenforschung)

Cite this

Ramskogler, C., Krumphals, A., & Sommitsch, C. (2011). Mikrostrukturentwicklung beim Friction Stir Processing von Ti-6Al-4V. Poster session presented at ASMET Forum, Leoben, Austria, .