Original language | English |
---|---|
Title of host publication | Materials Science |
Place of Publication | Wien |
Publisher | Facultas |
Pages | 257-258 |
ISBN (Print) | 978-3-85125-062-6 |
DOIs | |
Publication status | Published - 2009 |