Effect of weld defects on the fatigue strength of ultra high-strength steels

  • Markus J. Ottersböck (Speaker)
  • Leitner, M. (Contributor)
  • Michael Stoschka (Contributor)
  • Wilhelm Maurer (Contributor)

Activity: Talk or presentationTalk at conference or symposiumScience to science

Period2016
Event title18th International Colloquium on Mechanical Fatigue of Metals : ICMFM 2016
Event typeConference