New quantitative microstructural characterisation on creep tested welded joints

Publikation: Beitrag in Buch/Bericht/KonferenzbandBeitrag in einem KonferenzbandForschungBegutachtung

Originalspracheenglisch
Titel6th Int. Conference on Trends in Welding Research
ErscheinungsortPine Mountain, Georgia
Herausgeber (Verlag)ASM International
Seiten724-729
Band6
ISBN (Print)0-87170-627-X
PublikationsstatusVeröffentlicht - 2003
VeranstaltungInternational Conference on Trends in Welding Research - Pine Mountain, USA / Vereinigte Staaten
Dauer: 15 Apr 200219 Apr 2002

Publikationsreihe

NameTrends in Welding Research
Herausgeber (Verlag)ASM International

Konferenz

KonferenzInternational Conference on Trends in Welding Research
LandUSA / Vereinigte Staaten
OrtPine Mountain
Zeitraum15/04/0219/04/02

Dies zitieren

Letofsky, E., & Cerjak, H-H. (2003). New quantitative microstructural characterisation on creep tested welded joints. in 6th Int. Conference on Trends in Welding Research (Band 6, S. 724-729). (Trends in Welding Research). Pine Mountain, Georgia: ASM International.

New quantitative microstructural characterisation on creep tested welded joints. / Letofsky, Ernst; Cerjak, Horst-Hannes.

6th Int. Conference on Trends in Welding Research. Band 6 Pine Mountain, Georgia : ASM International, 2003. S. 724-729 (Trends in Welding Research).

Publikation: Beitrag in Buch/Bericht/KonferenzbandBeitrag in einem KonferenzbandForschungBegutachtung

Letofsky, E & Cerjak, H-H 2003, New quantitative microstructural characterisation on creep tested welded joints. in 6th Int. Conference on Trends in Welding Research. Bd. 6, Trends in Welding Research, ASM International, Pine Mountain, Georgia, S. 724-729, Pine Mountain, USA / Vereinigte Staaten, 15/04/02.
Letofsky E, Cerjak H-H. New quantitative microstructural characterisation on creep tested welded joints. in 6th Int. Conference on Trends in Welding Research. Band 6. Pine Mountain, Georgia: ASM International. 2003. S. 724-729. (Trends in Welding Research).
Letofsky, Ernst ; Cerjak, Horst-Hannes. / New quantitative microstructural characterisation on creep tested welded joints. 6th Int. Conference on Trends in Welding Research. Band 6 Pine Mountain, Georgia : ASM International, 2003. S. 724-729 (Trends in Welding Research).
@inproceedings{7427879e8a7f4ecab354bb6f246a850f,
title = "New quantitative microstructural characterisation on creep tested welded joints",
author = "Ernst Letofsky and Horst-Hannes Cerjak",
year = "2003",
language = "English",
isbn = "0-87170-627-X",
volume = "6",
series = "Trends in Welding Research",
publisher = "ASM International",
pages = "724--729",
booktitle = "6th Int. Conference on Trends in Welding Research",
address = "United States",

}

TY - GEN

T1 - New quantitative microstructural characterisation on creep tested welded joints

AU - Letofsky, Ernst

AU - Cerjak, Horst-Hannes

PY - 2003

Y1 - 2003

M3 - Conference contribution

SN - 0-87170-627-X

VL - 6

T3 - Trends in Welding Research

SP - 724

EP - 729

BT - 6th Int. Conference on Trends in Welding Research

PB - ASM International

CY - Pine Mountain, Georgia

ER -