Erratum to: Lifetime of Positrons in Nanostructured Nonstoichiometric Silver Sulfide Ag2–δS (JETP Letters, (2018), 107, 1, (4-9), 10.1134/S0021364018010095)

A. A. Rempel, S. I. Sadovnikov, G. Klinser, W. Sprengel

Publikation: Beitrag in einer FachzeitschriftDiskussionForschungBegutachtung

Abstract

Page 5, Table 1, row 2 should read: *2 − − − 3.60 ± 0.12 230 ± 10 175 ± 10 219 ± 5 69 ± 6 330 ± 12 31 ± 6 Page 5, left column, last paragraph should read: The lifetime of positrons in silver sulfide samples with different average sizes of nanoparticles was measured at the Institute of Materials Physics, Graz University of Technology (Austria), on a γγ fast—fast coincidence spectrometer using 22NaCl radioactive salt deposited on a 5-μm aluminum foil as a source of positrons. To record the positron annihilation spectra, we prepared a source with an activity of 1−2 MBq, which was placed between two silver sulfide tablets.

Originalspracheenglisch
Seitenumfang1
FachzeitschriftJETP letters
Jahrgang107
Ausgabenummer8
DOIs
PublikationsstatusVeröffentlicht - 1 Apr 2018

Fingerprint

sulfides
positrons
silver
life (durability)
Austria
tablets
positron annihilation
foils
spectrometers
salts
aluminum
nanoparticles
physics

ASJC Scopus subject areas

  • !!Physics and Astronomy (miscellaneous)

Dies zitieren

Erratum to : Lifetime of Positrons in Nanostructured Nonstoichiometric Silver Sulfide Ag2–δS (JETP Letters, (2018), 107, 1, (4-9), 10.1134/S0021364018010095). / Rempel, A. A.; Sadovnikov, S. I.; Klinser, G.; Sprengel, W.

in: JETP letters, Jahrgang 107, Nr. 8, 01.04.2018.

Publikation: Beitrag in einer FachzeitschriftDiskussionForschungBegutachtung

@article{41d4d35cfcb5433eac3ad6901bc887cc,
title = "Erratum to: Lifetime of Positrons in Nanostructured Nonstoichiometric Silver Sulfide Ag2–δS (JETP Letters, (2018), 107, 1, (4-9), 10.1134/S0021364018010095)",
abstract = "Page 5, Table 1, row 2 should read: *2 − − − 3.60 ± 0.12 230 ± 10 175 ± 10 219 ± 5 69 ± 6 330 ± 12 31 ± 6 Page 5, left column, last paragraph should read: The lifetime of positrons in silver sulfide samples with different average sizes of nanoparticles was measured at the Institute of Materials Physics, Graz University of Technology (Austria), on a γγ fast—fast coincidence spectrometer using 22NaCl radioactive salt deposited on a 5-μm aluminum foil as a source of positrons. To record the positron annihilation spectra, we prepared a source with an activity of 1−2 MBq, which was placed between two silver sulfide tablets.",
author = "Rempel, {A. A.} and Sadovnikov, {S. I.} and G. Klinser and W. Sprengel",
year = "2018",
month = "4",
day = "1",
doi = "10.1134/S0021364018080131",
language = "English",
volume = "107",
journal = "JETP letters",
issn = "0021-3640",
publisher = "Maik Nauka-Interperiodica Publishing",
number = "8",

}

TY - JOUR

T1 - Erratum to

T2 - Lifetime of Positrons in Nanostructured Nonstoichiometric Silver Sulfide Ag2–δS (JETP Letters, (2018), 107, 1, (4-9), 10.1134/S0021364018010095)

AU - Rempel, A. A.

AU - Sadovnikov, S. I.

AU - Klinser, G.

AU - Sprengel, W.

PY - 2018/4/1

Y1 - 2018/4/1

N2 - Page 5, Table 1, row 2 should read: *2 − − − 3.60 ± 0.12 230 ± 10 175 ± 10 219 ± 5 69 ± 6 330 ± 12 31 ± 6 Page 5, left column, last paragraph should read: The lifetime of positrons in silver sulfide samples with different average sizes of nanoparticles was measured at the Institute of Materials Physics, Graz University of Technology (Austria), on a γγ fast—fast coincidence spectrometer using 22NaCl radioactive salt deposited on a 5-μm aluminum foil as a source of positrons. To record the positron annihilation spectra, we prepared a source with an activity of 1−2 MBq, which was placed between two silver sulfide tablets.

AB - Page 5, Table 1, row 2 should read: *2 − − − 3.60 ± 0.12 230 ± 10 175 ± 10 219 ± 5 69 ± 6 330 ± 12 31 ± 6 Page 5, left column, last paragraph should read: The lifetime of positrons in silver sulfide samples with different average sizes of nanoparticles was measured at the Institute of Materials Physics, Graz University of Technology (Austria), on a γγ fast—fast coincidence spectrometer using 22NaCl radioactive salt deposited on a 5-μm aluminum foil as a source of positrons. To record the positron annihilation spectra, we prepared a source with an activity of 1−2 MBq, which was placed between two silver sulfide tablets.

UR - http://www.scopus.com/inward/record.url?scp=85049235846&partnerID=8YFLogxK

U2 - 10.1134/S0021364018080131

DO - 10.1134/S0021364018080131

M3 - Comment/debate

VL - 107

JO - JETP letters

JF - JETP letters

SN - 0021-3640

IS - 8

ER -