Microstructure and mechanical properties of the superalloy ATI Allvac 718Plus

Gerald A. Zickler, Ronald Schnitzer, Rene Radis, Rainer Hochfellner, Ralf Schweins, Martin Stockinger, Harald Leitner

Research output: Contribution to journalArticlepeer-review

Original languageEnglish
Pages (from-to)295-303
JournalMaterials Science and Engineering / A
Volume523
Publication statusPublished - 2009