Long-termdegradation of La0.6Sr0.4Co0.2Fe0.8O3-δ IT-SOFC cathodes due to silicon poisoning

Martin Perz, Edith Bucher, Christian Gspan, Jörg Waldhäusl, Ferdinand Hofer, Werner Sitte

Research output: Contribution to journalArticleResearchpeer-review

Original languageEnglish
Article numberhttp://dx.doi.org/10.1016/j.ssi.2016.01.005
Pages (from-to)22-27
JournalSolid State Ionics
Volume288
DOIs
Publication statusPublished - 2016

ASJC Scopus subject areas

  • Materials Science(all)

Fields of Expertise

  • Advanced Materials Science

Treatment code (Nähere Zuordnung)

  • Basic - Fundamental (Grundlagenforschung)

Cite this