In Situ Investigation of the Oxidation of Cobalt-Base Superalloys in the Environmental Scanning Electron Microscope

M. Weiser, Angelika Reichmann, Mihaela Albu, S. Virtanen, Peter Pölt

Research output: Contribution to journalArticle

Original languageEnglish
Pages (from-to)1158-1167
JournalAdvanced Engineering Materials
Volume17
Issue number8
DOIs
Publication statusPublished - 2015