Hot deformation behavior of a ni‐based superalloy with suppressed precipitation

Franco Lizzi, Kashyap Pradeep, Aleksandar Stanojevic, Silvana Sommadossi, Maria Cecilia Poletti*

*Corresponding author for this work

Research output: Contribution to journalArticle

Fingerprint Dive into the research topics of 'Hot deformation behavior of a ni‐based superalloy with suppressed precipitation'. Together they form a unique fingerprint.

Chemical Compounds

Engineering & Materials Science