Electrochemical characterization and surface analysis of bulk amorphous alloys in aqueous solutions at different pH

David L Cocke, D.G. Naugle, H McWhinney, Robert Schennach

Research output: Contribution to conference(Old data) Lecture or Presentation

Original languageEnglish
Publication statusPublished - 2 Oct 2000
Event47th International Symposium of the American Vacuum Society - Boston, MA, United States
Duration: 2 Oct 20006 Oct 2000

Conference

Conference47th International Symposium of the American Vacuum Society
CountryUnited States
CityBoston, MA
Period2/10/006/10/00

Treatment code (Nähere Zuordnung)

  • Basic - Fundamental (Grundlagenforschung)