Differential Scanning Calorimetry and Thermo Gravimetry with In-Situ Online Mass Spectrometry Studies on Lithium Iron Phosphate Cathodes and Carbon Anodes

Roland Hohl, Harald Kren, Bernd Fuchsbichler, Christoph Stangl, Cornelia Bayer, Colin God, Otto Fruhwirth, Martin Schmuck, Stefan Koller, Michael Sternad