Analysis of low-stress creep testing data and its implication on the life-time prediction for 9-12% Cr steels

Christian Schlacher, Peter Mayr

Research output: Contribution to conference(Old data) Lecture or Presentation

Original languageGerman
Publication statusPublished - 27 May 2012
EventCreep 2012 - Kyoto, Japan
Duration: 27 May 201231 May 2012

Conference

ConferenceCreep 2012
CountryJapan
CityKyoto
Period27/05/1231/05/12

Fields of Expertise

  • Advanced Materials Science

Treatment code (Nähere Zuordnung)

  • Basic - Fundamental (Grundlagenforschung)
  • Theoretical
  • Experimental

Cite this