Pitting corrosion behaviourof stainless steel AISI 304 with different tinting colours

Activity: Talk or presentationTalk at conference or symposiumScience to science

Period25 May 2017
Event titleESSC & DUPLEX 2017: 9th European Stainless Steel Conference - Science & Market / 5th European Duplex Stainless Steel Conference & Exhibition
Event typeConference
LocationBergamo, Italy

Fields of Expertise

  • Advanced Materials Science