The Precipitation Behavior of Superalloy ATI Allvac 718 Plus

Gerald A. Zickler, Rene Radis, Ronald Schnitzer, Ernst Kozeschnik, Martin Stockinger, Harald Leitner

Publikation: Beitrag in einer FachzeitschriftArtikelForschungBegutachtung

Originalspracheenglisch
Seiten (von - bis)176-183
FachzeitschriftAdvanced Engineering Materials
Jahrgang12
PublikationsstatusVeröffentlicht - 2010

Treatment code (Nähere Zuordnung)

  • Application
  • Theoretical
  • Experimental

Dies zitieren

Zickler, G. A., Radis, R., Schnitzer, R., Kozeschnik, E., Stockinger, M., & Leitner, H. (2010). The Precipitation Behavior of Superalloy ATI Allvac 718 Plus. Advanced Engineering Materials, 12, 176-183.

The Precipitation Behavior of Superalloy ATI Allvac 718 Plus. / Zickler, Gerald A.; Radis, Rene; Schnitzer, Ronald; Kozeschnik, Ernst; Stockinger, Martin; Leitner, Harald.

in: Advanced Engineering Materials, Jahrgang 12, 2010, S. 176-183.

Publikation: Beitrag in einer FachzeitschriftArtikelForschungBegutachtung

Zickler, GA, Radis, R, Schnitzer, R, Kozeschnik, E, Stockinger, M & Leitner, H 2010, 'The Precipitation Behavior of Superalloy ATI Allvac 718 Plus' Advanced Engineering Materials, Jg. 12, S. 176-183.
Zickler GA, Radis R, Schnitzer R, Kozeschnik E, Stockinger M, Leitner H. The Precipitation Behavior of Superalloy ATI Allvac 718 Plus. Advanced Engineering Materials. 2010;12:176-183.
Zickler, Gerald A. ; Radis, Rene ; Schnitzer, Ronald ; Kozeschnik, Ernst ; Stockinger, Martin ; Leitner, Harald. / The Precipitation Behavior of Superalloy ATI Allvac 718 Plus. in: Advanced Engineering Materials. 2010 ; Jahrgang 12. S. 176-183.
@article{f4fcd3a981314815bd72d77fbf4d0d1a,
title = "The Precipitation Behavior of Superalloy ATI Allvac 718 Plus",
author = "Zickler, {Gerald A.} and Rene Radis and Ronald Schnitzer and Ernst Kozeschnik and Martin Stockinger and Harald Leitner",
year = "2010",
language = "English",
volume = "12",
pages = "176--183",
journal = "Advanced Engineering Materials",
issn = "1438-1656",
publisher = "Wiley-VCH",

}

TY - JOUR

T1 - The Precipitation Behavior of Superalloy ATI Allvac 718 Plus

AU - Zickler, Gerald A.

AU - Radis, Rene

AU - Schnitzer, Ronald

AU - Kozeschnik, Ernst

AU - Stockinger, Martin

AU - Leitner, Harald

PY - 2010

Y1 - 2010

M3 - Article

VL - 12

SP - 176

EP - 183

JO - Advanced Engineering Materials

JF - Advanced Engineering Materials

SN - 1438-1656

ER -