Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation

Roman Pschera, Christof Sommitsch, Gerald Winter

Publikation: KonferenzbeitragPosterForschung

Originalspracheenglisch
PublikationsstatusVeröffentlicht - 2007
VeranstaltungEuropean Congress and Exhibition on Advanced Materials and Processes - Nürnberg, Deutschland
Dauer: 10 Sep 200713 Sep 2007

Konferenz

KonferenzEuropean Congress and Exhibition on Advanced Materials and Processes
KurztitelEuromat 2007
LandDeutschland
OrtNürnberg
Zeitraum10/09/0713/09/07

Dies zitieren

Pschera, R., Sommitsch, C., & Winter, G. (2007). Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation. Postersitzung präsentiert bei European Congress and Exhibition on Advanced Materials and Processes, Nürnberg, Deutschland.

Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation. / Pschera, Roman; Sommitsch, Christof; Winter, Gerald.

2007. Postersitzung präsentiert bei European Congress and Exhibition on Advanced Materials and Processes, Nürnberg, Deutschland.

Publikation: KonferenzbeitragPosterForschung

Pschera, R, Sommitsch, C & Winter, G 2007, 'Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation' European Congress and Exhibition on Advanced Materials and Processes, Nürnberg, Deutschland, 10/09/07 - 13/09/07, .
Pschera R, Sommitsch C, Winter G. Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation. 2007. Postersitzung präsentiert bei European Congress and Exhibition on Advanced Materials and Processes, Nürnberg, Deutschland.
Pschera, Roman ; Sommitsch, Christof ; Winter, Gerald. / Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation. Postersitzung präsentiert bei European Congress and Exhibition on Advanced Materials and Processes, Nürnberg, Deutschland.
@conference{05db937631d74510986d8c8b6b199293,
title = "Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation",
author = "Roman Pschera and Christof Sommitsch and Gerald Winter",
year = "2007",
language = "English",
note = "Euromat 2007, Euromat 2007 ; Conference date: 10-09-2007 Through 13-09-2007",

}

TY - CONF

T1 - Optical Surface Analysis of Steel during Hot Compression: A Test to Determine Crack Initiation

AU - Pschera, Roman

AU - Sommitsch, Christof

AU - Winter, Gerald

PY - 2007

Y1 - 2007

M3 - Poster

ER -