Influence of the electrolyte composition on the capacity fade of lithium alloy anodes

Markus Robert Wagner, Kai-Christian Möller, Jürgen Besenhard, Martin Winter

Publikation: Beitrag in Buch/Bericht/KonferenzbandBeitrag in einem KonferenzbandForschung

Originalspracheenglisch
Titel4th Advanced Batteries and Accumulators (A.B.A.)
Herausgeber (Verlag).
Seiten48-48
ISBN (Print)80-214-2298-X
PublikationsstatusVeröffentlicht - 2003
Veranstaltung4th Advanced Batteries and Accumulators (A.B.A.) - Brno, Tschechische Republik
Dauer: 15 Jun 200319 Jun 2003

Konferenz

Konferenz4th Advanced Batteries and Accumulators (A.B.A.)
LandTschechische Republik
OrtBrno
Zeitraum15/06/0319/06/03

Dies zitieren

Wagner, M. R., Möller, K-C., Besenhard, J., & Winter, M. (2003). Influence of the electrolyte composition on the capacity fade of lithium alloy anodes. in 4th Advanced Batteries and Accumulators (A.B.A.) (S. 48-48). ..

Influence of the electrolyte composition on the capacity fade of lithium alloy anodes. / Wagner, Markus Robert; Möller, Kai-Christian; Besenhard, Jürgen; Winter, Martin.

4th Advanced Batteries and Accumulators (A.B.A.). ., 2003. S. 48-48.

Publikation: Beitrag in Buch/Bericht/KonferenzbandBeitrag in einem KonferenzbandForschung

Wagner, MR, Möller, K-C, Besenhard, J & Winter, M 2003, Influence of the electrolyte composition on the capacity fade of lithium alloy anodes. in 4th Advanced Batteries and Accumulators (A.B.A.). ., S. 48-48, Brno, Tschechische Republik, 15/06/03.
Wagner MR, Möller K-C, Besenhard J, Winter M. Influence of the electrolyte composition on the capacity fade of lithium alloy anodes. in 4th Advanced Batteries and Accumulators (A.B.A.). . 2003. S. 48-48
Wagner, Markus Robert ; Möller, Kai-Christian ; Besenhard, Jürgen ; Winter, Martin. / Influence of the electrolyte composition on the capacity fade of lithium alloy anodes. 4th Advanced Batteries and Accumulators (A.B.A.). ., 2003. S. 48-48
@inproceedings{00d5e42695554ec29b358774a816b7b3,
title = "Influence of the electrolyte composition on the capacity fade of lithium alloy anodes",
author = "Wagner, {Markus Robert} and Kai-Christian M{\"o}ller and J{\"u}rgen Besenhard and Martin Winter",
year = "2003",
language = "English",
isbn = "80-214-2298-X",
pages = "48--48",
booktitle = "4th Advanced Batteries and Accumulators (A.B.A.)",
publisher = ".",

}

TY - GEN

T1 - Influence of the electrolyte composition on the capacity fade of lithium alloy anodes

AU - Wagner, Markus Robert

AU - Möller, Kai-Christian

AU - Besenhard, Jürgen

AU - Winter, Martin

PY - 2003

Y1 - 2003

M3 - Conference contribution

SN - 80-214-2298-X

SP - 48

EP - 48

BT - 4th Advanced Batteries and Accumulators (A.B.A.)

PB - .

ER -