title = "Characterization of δ-phase in superalloy Allvac 718PlusTM",
author = "Christoph Stotter and Christof Sommitsch and Julian Wagner and Leitner Harald and Ilse Letofsky-Papst and Prantl Werner and Martin Stockinger and Zickler, {Gerald A.}",
year = "2008",
doi = "10.3139/146.101648",
language = "English",
volume = "4",
pages = "376--380",
journal = "International Journal of Materials Research ",
issn = "2195-8556",
publisher = "deGruyter",
number = "99",
}